FAQ: Shore durometers

What is a durometer?

The durometer is a measuring instrument for technical hardness testing of rubber and plastic articles and of non-metallic materials.

What is meant by hardness?

Hardness is understood as the resistance to penetration of an indenter with a specific geometric shape under a defined force into the sample. The indentation depth is measured and displayed in analogue or digital form.

What is meant by Shore?

Hardness is understood as the resistance to penetration of an indenter with a specific geometric shape under a defined force into the sample. The indentation depth is measured and displayed in analogue or digital form.

Which parts can be measured with Shore?

From soft silicones to elastomers and plastics. Material thickness and material width are also decisive.

For which applications are the variants used?
  • Durometer A: soft rubber, elastomers, natural rubber…
  • Durometer AO: foams, steering wheels, interior trim, automotive…
  • Durometer D: hard rubber, rigid thermoplastics…
  • Durometer B: hard elastomers where the hardness lies between Shore A and Shore D…
  • Durometer C: medium-hard elastomers…
  • Durometer DO: dense-grained materials, textile fabrics…
  • Durometer O: soft elastomers, textile fabrics…
  • Durometer OO: foam, moss and cellular rubber…
How large is the indentation depth?

Depending on the variant and in the unloaded state (display 0 Shore), the indenter protrudes 2.5 mm beyond the pressure foot. If the hardness tester is pressed onto a ground steel plate, the display shows 100 Shore (no penetration into the elastomer).

What geometry do the indenters have?
  • Durometer A and C: Ø0.79 mm / 35° / Ø1.25
  • Durometer D and B: R0.1 / 30° / Ø1.25
  • Durometer AO: Ø5 mm
  • Durometer DO, O and OO: Ø2.38 mm
What is the max. spring force (at 100 Shore)?

Every Shore hardness tester has a spring. This spring produces the required force, i.e. each indentation depth has an assigned force.

  • Durometer OO: 1.11 N
  • Durometer A, AO, B and O: 8.05 N
  • Durometer D, C and DO: 44.5 N
  • Durometer Asker C: 8.39 N
In which measuring range should the durometers be used?

The measuring range is from 0 to 100 Shore. Values from 0 to 10 and from 90 to 100 should not be used. If values occur in these ranges, a different Shore hardness scale is used.

Which durometer scale can be used to measure shoe soles?

Usually Shore A.

What material thickness is required?

>6 mm or layers 2 mm + 2 mm + 2 mm = 6 mm. If the test piece is e.g. 1.5 mm thick, it cannot be measured using the Shore method. The indenter protrudes 2.5 mm from the pressure foot in the unloaded state; in this case the substrate would influence the measurement.

What do I need to consider regarding the measuring time?

The measuring time begins after the pressure foot has been placed. There are different measuring times depending on the standard, i.e. readings from different standards can only be compared to a limited extent. ASTM D 2240 hardness values are higher than ISO 7619-1 hardness values. With ISO 7619-1 the indenter has more time to penetrate the material. If the readings are to be comparable, the same time must always be used.

What is a drag pointer?

The regular pointer always shows the current hardness value. If the knurled screw in the centre of the dial is turned anticlockwise, the drag pointer is set to 0. During a hardness measurement, the regular pointer takes the drag pointer with it up to the maximum hardness value. The drag pointer then remains in this position (e.g. 62 Shore A). The regular pointer may show a lower value (e.g. 59 Shore A) because the material flows (depending on material and measuring time).

Why should a test stand be used for Shore hardness testing?

Testing by hand: the contact force of the durometer on the sample is produced by hand (mass of hardness tester + hand force). Subjective measuring errors caused by incorrect contact force or non-vertical measurements are possible, i.e. the readings vary more – larger deviations (the range is greater).

Test stand: when using a test stand, the hardness tester is lowered smoothly with a constant test force – using a toggle lever. The hardness tester + holder + shaft + weight represent the mass. An additional weight of 4000 g is required for Shore D.

How often should calibration be carried out?

Shore calibration is described in ISO 18898 (also ASTM D 2240 for hardness testers not described in ISO 18898). The minimum requirements for the measuring equipment are also described (in ISO 18898). During calibration, the geometry of the indenter and pressure foot, the measuring force (spring) and the measuring travel are checked. We recommend annual calibration.

How do I store the durometer?

The durometer should be stored in a clean, dry place out of direct sunlight, ideally in the case provided for this purpose.

How can I avoid measuring errors?
  • Before measuring, check whether the durometer is suitable for the material of the workpiece to be tested. The reading should be between 10 and 90.
  • The ambient temperature, the temperature of the workpiece and the temperature of the durometer should ideally be 23°C.
  • The specified material thickness must not be undercut.
  • The surface of the test piece must be clean and flat and have two parallel surfaces.
  • The measuring direction is vertical from top to bottom. Make sure that the contact surface of the durometer is always parallel to the surface of the test piece.
  • The placing and measuring speed should be about 2.5 mm/s (max. 3.2 mm/s according to the standard).
  • The measuring time must be observed.
  • If several measurements are taken on one test piece, each measuring position may only be used once, i.e. the workpiece or the durometer is moved after each measurement.
  • If the durometer has been used improperly, it must be checked or recalibrated.